| ALLOY | UNS NO. | Condition | Yield Strength (0.2%) (Ksi) |
Tensile Strength (Ksi) |
Elongation (%) |
Reduction in Area (%) |
Hardness | NACE MR0175 Listed |
|---|---|---|---|---|---|---|---|---|
| Grade 2 | R50400 | Anneal | 40 | 50 | 20 | 30 | 100Rb Max | Yes |
| Grade 7 | R52400 | Anneal | 40 | 50 | 20 | 25 | 98-102Rb | No |
| Grade 12 | R53400 | Anneal | 50 | 70 | 18 | 25 | 92Rb Max | Yes |
| Grade 9 (3AL-2.5V) | R56320 | Anneal | 70 | 90 | 15 | - | 24-28Rc | No |
| Grade 5 (6AL-4V) | R56400 | Anneal | 120 | 130 | 10 | 20 | 28-34Rc | No |
| 6AL-6V-2Sn | R56620 | Anneal | 135-160 | 147-170 | 8-12 | 15-30 | 28-36Rc | No |
| 6AL-2Sn-4Zr-6Mo | R56260 | Solution Treat & Age |
135-165 | 145-175 | 6-20 | 10-35 | 45Rc Max | Yes |
| Grade 19 (Beta-C) | R58640 | Solution Treat & Age |
115-180 | 120-190 | 5-20 | 10-35 | 42Rc Max | Yes |